[DPRG] semi-OT: sealed case VS conformal coating
Subject: [DPRG] semi-OT: sealed case VS conformal coating
From: Mike Dodson
madodson at gmail.com
Date: Wed Jan 9 16:50:57 CST 2008
LOOK AT TECHSPRAYS WEBSITE FOR THE SPECS, BUT WE ONLY HAVE TO DO A PARTIAL
BAKE.
JUST ENOUGH FOR YOU TO HANDLE THEM. AMBIENT AIR DRY IS OK, JUST TAKES
LONGER.
I WILL SAY THAT THE SR DRIES FASTER? AND IS EASIER TO REPAIR THRU THE
COATING.
MIKE
On Jan 9, 2008 4:32 PM, Sluggy! <sluggy9912 at swbell.net> wrote:
> --- Mike Dodson <madodson at gmail.com> wrote:
>
> > I HAVE ON HAND TECHSPRAY BOTH FINE-L-KOTE SR, AND
> > HT. BOTH ARE SILICONE
> > BASED.
>
> What is the difference between them?
>
> > WE WILL HAVE TO BAKE THE BOARD FOR A WHILE TO DRY,
>
> How much baking does it take?
>
> Sluggy!
>
> ---
>
> "The idea that unicycling is intrinsically funny does not explain the
> findings." Professor Sam Shuster.
> _______________________________________________
> DPRGlist mailing list
> DPRGlist at dprg.org
> http://list.dprg.org/mailman/listinfo/dprglist
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: http://list.dprg.org/pipermail/dprglist/attachments/20080109/37facc67/attachment.html
More information about the DPRG mailing list
|